(!)Due to Microsoft's end of support for Internet Explorer 11 on 15/06/2022, this site does not support the recommended environment.

  • Pembayaran dengan kartu kredit untuk sementara tidak tersedia karena kendala sistem. Sementara waktu Anda dapat meggunakan metode Pembayaran di Muka atau QRIS. Untuk informasi lebih lanjut, silakan hubungi Customer Service : TEL: 021-8984-0008 E-mail: cs@misumi.co.id. WA: 08118984008. Kami mohon maaf atas ketidaknyamanan yang terjadi.
    Credit card payments are temporarily unavailable due to system issues. Meanwhile, you can use the Advance Payment method or QRIS. For further information, please contact Customer Service: TEL: 021-8984-0008 E-mail: cs@misumi.co.id. WA: 08118984008. We apologize for any inconvenience caused.
  • Sehubungan dengan adanya Peraturan Baru Kementerian Perdagangan No.36 Tahun 2023 tentang Pembatasan Impor Barang, MISUMI Indonesia melakukan tindakan pencegahan. Lihat informasi detailnya di sini
    Due to New Regulation of Ministry Of Trade No.36 of 2023 concerning retrictions on imports of goods, MISUMI Indonesia do precautions measure. See detail information here
  • Nomor telepon alternatif Kontak Layanan Pelanggan : 021-29182911| 021-29182991 | 021-29182997 | 021-29182998
    Alternative telephone number Contact Customer Service: 021-29182911 | 021-29182991 | 021-29182997 | 021-29182998

Welding gauge AWG-10

Welding gauge AWG-10

Click this image to zoom it.

Move the mouse over the image to zoom

Dedicated analog type gauge for measuring throat depth of fillet and height of excess weld metal. An essential item for welding processes.
[Features]
· Made of stainless steel for simple anti-rust treatment.
· Beveling angle: 60°, 70°, 80°, 90°.
· Fillet throat thickness: 11 mm.
· Height of excess weld metal: 8 mm.
· Instrument difference: ±0.2 mm.
· Minimum read value: 0.1 mm.
[Applications]
· Used to determine the size of weld overlay and fillet.

PDF

Japanese Only

Part Number

Configured Part Number is shown.

AWG-10

What is welding gauge

Welding gauge is used to measure and check size of welded part throat
thickness required strength split that may casue damage irregularity of
under-cut and overlap etc.
 

Terms of welding

  • Throat thickness
    The thickness from welded portion at triangular cross-section when welding two faces at 90°.
  • Arc strike
    The arc that occurred to parts other than welding base metal when working on arc welding.
  • Pit
    Blow hole on surface due to poor welding.
  • Bead
    A belt shape rises after working on welding.
  • Under-Cut
    The irregular groove at the toe of a rod in the welding base metal.
  • Overlap
    The heap results from miss welding of the base metal.


Instructions for inspection

Inspection itemsPictureinstruction for measuring
Reasons of welding crack
1.Surface crack
on bead
Visual inspectin in priciple
Inspection of exterior and shape on welding bead
2.Pit on welding bead surfaceVisual inspection
3.Unevenness on welding bead surface
4.Under-cut
5.OverlapVisual inspection
6.Size of corner buds (Lack of throat thickness • foot length of fillet)
7.Excessive buds from groove welding
Others
8.Arc strikeVisual inspection
Part Number
AWG-10
Part NumberMinimum order quantityVolume DiscountDays to Ship
1 Piece(s) 30 Day(s)

Loading...

  1. 1
 

Basic Information

Measuring Range(mm) 11 Minimum Read Value(mm) 0.1 Dimensions Measurement Accuracy(mm) ±0.2
Measuring bevel angle / groove angle(°) 60°、70°、80°、90° Mass(g) 80 Material Stainless Steel
Feature 1 · Made with stainless steel for easy anti-rust processing Use Weld Overlay, Fillet Size

Please check the type/dimensions/specifications of the part AWG-10 in the Welding gauge AWG-10 series.

Tech Support

Factory Automation, Electronics, Tools, & MRO (Maintenance, Repair and Operations)
Tel:021-8990-4102 / FAX:021-8990-5803
8:30am - 5:30pm (Monday - Friday)